Some bottom layer separation issues but otherwise I’m impressed with the increase in detail for 20 micron layers when I normally print at 50. Resin is the pink AC soy based resin, bottom layers were exposed for 40 seconds and regular layers for 6, do any of y’all have any suggestions for adjusting the print settings? I think I need to increase the quantity of bottom layers and lower the bottom layer expose to maybe 10 or 20 seconds but I’d like to hear your thoughts