Hi all , I have been using the photon for a couple of months now and have been pleased with the results.I changed my resin to Bluecast X5. as i want to cast the models. Which i have done successfully .My settings so far have been 100 seconds for the base layers of 6. My normal exposure has been 11 to 15. I have just printed using the resin calibration from photonsters using the resin-test-25u.B150.6-60 for slow resins . The result has given me a best column of 8 to 9. Question does this mean i have to multiply 8 or 9 by 6 to give me my normal exposure? 48 seconds seems to be way over what i have used so far. Whats your thoughts chaps.
翻譯年糕
Zena Andreou
2019-02-03 22:41:16
Zena Andreou
2019-02-03 22:45:15