Aside from the 100k thermistor, are there other consumable parts I should stock up on to reduce downtime?
翻譯年糕
Clarence Lee
2016-03-27 17:58:15
Noel Singson
2016-03-27 18:24:08
Hahaha I was afraid someone would say that.
Clarence Lee
2016-03-27 18:56:46
When you are maintenance your hotend, you would like to install another when your are working on it. Much shorter down time.
Birk Binnard
2016-03-27 23:16:54
PTFE tubing for inside the hot end. It is 3/2 mm OD/ID. Nozzle jams are usually the result of crystallized plastic stuck on the inside of the tube, or sometimes the tube just getting burned.