Could you guys help me with a few questions regarding the film please?
1. What causes permanent marks to develop on the FEP film?
After replacing the film, the first print on it succeeded, but had very loud peeling sounds, left permanent marks, and had a large layer of cured resin stuck to the bottom on two attempts. My film now has cloudy marks in the shape of the prints, and divots in the film itself.
2. How do I avoid marring the film when replacing it?
When replacing the film I used a bottlecap as in the video, but it left a small imperfection in the film that did not go away when tensioned.
3. What are the symptoms of a film that's too tight or too lose?
My factory film install seemed perfect, I didn't even tighten it when I got it. Now, as mentioned before, the peeling sounds are loud and it's marring easily. Does this mean my film is too tight or too loose?
翻譯年糕
Sen Kun
2019-01-13 16:03:03
Philipp Douglas
2019-01-13 16:22:57
Sen Kun
2019-01-13 16:23:56
Jean-François Meloche
2019-01-14 00:51:38
Philipp Douglas
2019-01-14 00:53:47