Smoothing/sealing PLA with Tetrahydrofuran

These links explain how the chemical Tetrahydrofuran can be used to smooth and/or seal PLA 3D printed parts just like Acetone does with ABS:

https://www.youtube.com/watch?v=KJYaqaUr7iw

http://www.protoparadigm.com/…/vapor-smoothing-and-polishi…/

Puchase it here: http://www.amazon.com/s/?field-keywords=tetrahydrofuran

There are other postings about this method that suggest some experimentation is needed, but it looks promising for PLA parts.

翻譯年糕

André Medborg
2015-08-28 12:15:21

During your search did you find any other names for this chemical? I live in Denmark and I haven't been able to locate it here. The closest thing I found was a fluid used preparing fancy nails.

Birk Binnard
2015-08-28 12:40:59

No, that name is all I looked for. It is a standard English chemical name and I have no idea what how how it might be translated into different languages. My guess is it would be about the same, but I really don't know.

Birk Binnard
2015-08-28 12:44:40

The chemical is also the major component of the sticky glue used to glue pieces of plastic pipe used for plumbing together. But I don't think this glue would work for smoothing PLA because it won't be nearly as volatile.

André Medborg
2015-08-28 14:30:17

Apparently the solvent is also called THF

Birk Binnard
2015-08-28 16:00:16

That sounds reasonable. Many chemicals here in the US have short names like that: DDT; 2-4-5-T; HF; TCE, etc.


原文網址 Артем Белькевич
2015-08-28 02:11:07


原文網址 丁耀
2015-08-28 00:19:16

陳明谷
2015-08-28 00:53:22

是拉緊又不會太緊

丁耀
2015-08-28 01:05:56

就是沒有135釐米也可以了?

高北熊
2015-08-28 02:16:37

135mm最適距離

葉世瑋
2015-08-28 07:02:11

以135cm為基準安裝,之後再調整皮帶張力

廖新弘
2015-08-28 08:31:24

你可以不要按照建議安裝,然後裝完後,再拆一次

劉武鑫
2015-08-28 08:44:08

我裝的時候量剛剛好135結果沒辦法鎖
還加到136ㄎㄎ

廖新弘
2015-08-28 08:57:28

其實+-1~2mm是可以接受,只是要調整皮帶的鬆緊,容許空間變小了

丁耀
2015-08-28 10:06:39

我裝在130了


原文網址 曾俊維
2015-08-27 20:37:44

向各位前輩請教一下
換了1.5版的kiss之後,覺得很難用。好多設定我看不懂。
我這幾頁設定有什麼可以改進的地方。讓列印的品質更好呢?

先問幾點我看不懂的
1.style中的右下角的gap,是什麼意思,改大改小有什麼差別呢?
2.support中多了好多數值,看不懂,有前輩可以幫忙翻譯一下嗎?
3.在printer中的speed,左方的loops是指印外圈的速度嗎?
4.在matl中的多了兩個三角向上的數值,那個是改什麼呢?

還請了解的前輩幫忙解答一下,小弟的英文實在是太破了,只用單字去翻,也還是有看沒有懂啊。

Clarence Lee
2015-08-27 20:57:29

就改了一個參數就切完先在kisslicer內看各層路徑去觀察效果,差別
1.style中的右下角的gap,是什麼意思,改大改小有什麼差別呢?
https://www.facebook.com/groups/atom3dp/permalink/1626660540905568/
2.support中多了好多數值,看不懂,有前輩可以幫忙翻譯一下嗎?
3.在printer中的speed,左方的loops是指印外圈的速度嗎?
perimeter才是外圈, loops是外圈以外的牆
4.在matl中的多了兩個三角向上的數值,那個是改什麼呢?
vP是Prime的速度, vS是Suck的速度
就是新的可以分開設定

Charlie Ting
2015-08-27 20:59:05

感覺大有長進耶,很多細微的控制都開出介面了~~~作者有用心!

建議你是遇到問題再來找關鍵參數,不然你對每個參數會產生什麼連帶影響,影響的狀況多大,會不會有交互影響,會一直處於一知半解。

我個人覺得 KISSlicer 它簡化了針對圖面的操作,而盡量用參數去控制輸出。但是,當功能越來越細,它的駕馭難度會變高,反而其他程式會比較簡單理解。所以,這個要看你的使用狀況跟經驗累積速度了。

Odinson Thor
2015-08-27 21:22:11

Charlie Ting
2015-08-27 21:37:23

關於 gap & depth, 我覺得要這樣看。就是必須把噴嘴口徑想像進來,甚至還有跳轉過程的熱堆積或溢料。
因此,我一般 gap 大概都在 0.1~0.2 跳,depth 則在 0~0.2 之間。印出來的狀態是看得出接縫,但摸不出接縫。

Charlie Ting
2015-08-27 21:40:26

關於 support 那部份,主要就是把幾種不同的支撐作更細節的設定,試圖避免支撐變成列印失敗的主因(拆不掉)或浪費太多材料及時間。但個人覺得,少開支撐才是王道 XDDDD。

林祐德
2015-08-27 22:10:11

出新版了??? 為何已有新版的手冊了???

林祐德
2015-08-27 22:15:52

下載地址,剛找到了,原來我一直用的是1-45版 https://www.dropbox.com/....../AABau30kpAP2BEY1tffRFeG......

林祐德
2015-08-27 22:26:25

這一版的,配非官方手冊比較搭,全英文慢慢啃就成功了。 http://3ntr.eu/....../2015/02/KISSlicer_manual_EN_080215.pdf

林祐德
2015-08-27 22:29:49

期待這次boxing day , pro key會特價~~~


原文網址 Rickey Yang
2015-08-27 19:00:27

https://www.zeczec.com/projects/atom2/updates/573
計畫更新#21
關於雷射模組

Charlie Ting
2015-08-27 19:12:47

官方的就是不一樣.....
不過好奇雷射模組是否包含 HUB ?
還有最大的雕刻面積是?

黃俊傑
2015-08-27 19:23:57

肝...沒跟到集資的! 已哭!

姜智勻
2015-08-27 19:41:08

等好久了

Estima Lin
2015-08-27 19:54:32

等好久+1…
蛋、蛋、蛋…就固A~

Lawrence Lee
2015-08-28 14:03:05

Charlie Ting , 雷射模組有包含鋁合金HUB, 球頭x6, 防鬆螺母x6。因為讓大家久等了所以才加碼,希望誠意有做足!:-)

Charlie Ting
2015-08-28 14:04:21

Lawrence Lee 這樣超有誠意的~~~料好實在!!!

Tz-Shiang Su
2015-08-30 13:01:00

想請問一下,點連結進不去,有人有同樣問題嗎?

廖新弘
2015-08-30 13:18:15

是的,我也有同樣問題

李穆
2015-08-30 13:28:19

我也進不去!

Estima Lin
2015-08-30 13:32:52

可以阿!

廖新弘
2015-08-30 13:33:57

那是手機不是電腦

Charlie Ting
2015-08-30 13:35:33

我用電腦看得到,但要登錄嘖嘖才行

Estima Lin
2015-08-30 13:36:35

本來就要登入了不是嗎?

Rickey Yang
2015-08-30 13:48:51

不知是否限制贊助者才能看到
所以要登入

Estima Lin
2015-08-30 13:50:40

是限制贊助者沒錯啊!

李穆
2015-08-30 13:50:40

妙的是我登入就跑回FB頁面了


原文網址 李木子
2015-08-27 18:59:35

作品分享,雙色列印

期待ATOM 雙噴頭推出

不用暫停換料換得這麼辛苦QQ

辛旻勳
2015-08-27 19:38:42

漂亮

李木子
2015-08-27 19:43:18

謝謝 ^_^

Vincent LM Yeh
2015-08-27 19:49:22

請教換料技巧!

李木子
2015-08-27 19:54:34

Vincent LM Yeh 可以來參考這篇喔!
http://diy3dprint.blogspot.tw/2014/02/blog-post_10.html

我是手動來換料
因為在"wait for user"狀態 只要一點按鈕就會繼續印,無法進入選單來auto換料,或許板上有其他先進,可以提供更好的方法來執行auto換料~


原文網址 Hawke ChienSheng Liu
2015-08-27 17:06:06

第一次玩KISSlicer的Vase,印一隻招財貓。它會有頓呆的現象,向同好們請教一下⋯⋯

Clarence Lee
2015-08-27 17:07:33

gcode 可以傳來看一下嗎?

Hawke ChienSheng Liu
2015-08-27 17:16:15

私訊給你了;另外 KISSlicer設定是這樣的:

Hawke ChienSheng Liu
2015-08-27 17:16:48

Hawke ChienSheng Liu
2015-08-27 17:17:17

Mark Chen
2015-08-27 17:18:45

沒有噸阿 回抽速度15 看起來就像世界停止了

Clarence Lee
2015-08-27 17:21:40

回抽速度跟印速搭不起來..冏.

Hawke ChienSheng Liu
2015-08-27 17:22:23

原來如此,謝謝指導

Charlie Ting
2015-08-27 17:55:18

回抽15,長度8,等於一回抽大概會停0。5秒左右,但 trigger 100mm,所以在大範圍印完時才會發生。

Clarence Lee
2015-08-27 18:06:58

這個很小..應該是換層, 換路徑時發生;p

Charlie Ting
2015-08-27 18:09:40

有觸發 de-string? 還是其他誤判?(覺得對 KISSlicer 的 output 要略帶保留)

林祐德
2015-08-27 19:55:47

看路徑哦~^^ 不過我可以說,有時kiss切的方式還滿奇怪的,明明這一層可以一筆印完並順利上升z再印下一層,但它就喜歡東跑跑印一點,西跑跑印一點,轉到別的切片又ok了。

曾俊維
2015-08-27 21:10:12

kiss這點真的很怪。

Birk Binnard
2015-08-28 03:23:39

Why is side facing fan not turning?


原文網址 Bobble Chang
2015-08-27 12:28:36

最近在印大面積物件碰到一個狀況,,列印第一層時圓盤中間可正常列印,外圍會印不出來,試著調高G29 Z+值,結果外圍可正常列印,中間因噴頭調高,印出一堆斷續面,感覺是盤子中低外高,不過之前印大面積都正常,請問有可能那邊出的問題?
另外想問有人印大件時會按暫停後再續印嗎?晚上印怕吵到別人@@,暫停再續印有要注意的地方嗎?感謝

廖新弘
2015-08-27 13:27:07

之前有人建議做G29時把速度調慢50%,可以增加G29測量穩定度

Bobble Chang
2015-08-27 13:58:26

有放慢50%,不過還是一樣

廖新弘
2015-08-27 14:13:29

那麼檢查一下玻璃夾具是否夾緊

Kyle Tseng
2015-08-27 14:24:29

https://atom3dp.squarespace.com/firstlayer/
先按照官網檢查一遍,另外"集線管"的部分在做G29時要避免拉扯或壓迫到噴頭的動作,應該會改善很多,校正完就可以把G29拿掉,除非有去動平台或機構,否則不需要每次列印都做一次校正。

Bobble Chang
2015-08-27 14:34:43

好的,我再檢查一下,謝謝

陳明谷
2015-08-28 11:22:26

有解嗎


原文網址 Adam Chen
2015-08-27 02:49:23

版上有人用過這款線材嗎?
感覺搭配耐火石膏 要自己翻錫應該是沒問題

陳明谷
2015-08-27 08:16:30

在想…會不會沒多久水溝就阻塞了

Adam Chen
2015-08-27 08:23:38

水溝是指噴頭嗎?

陳明谷
2015-08-27 09:33:42

下水道!水管!
低溫蠟融化後跟水流進水溝
被金屬管壁等東西碰觸降溫 …… 查看更多

Adam Chen
2015-08-27 09:50:18

應該是不會啦 脫蠟鑄造這個存在很久了 而且蠟和油脂的特性不同 只要ㄧ碰到水馬上就凝固了 油指在水中還是可以流動
而且脫蠟後在空氣中也是幾秒後就凝固了 要丟棄應該也是丟垃圾桶啊

陳明谷
2015-08-27 09:53:14

或是可以回收再使用!
蠟不像PLA或ABS需要那麼高要求

Adam Chen
2015-08-27 09:55:05

蒐集起來加熱融化後插根棉線當蠟燭 :D

林祐德
2015-08-27 19:47:46

為何不用一般材料先印外模,再拿來翻蠟就好? 在印外模時也可以順便知道哪裡有缺失?

Adam Chen
2015-08-27 19:49:25

有些造型無法翻模 所以會需要用鑄造的方式

林祐德
2015-08-27 19:51:36

那麼無法翻模的樣品,是否給CAD檔會比較直接點? SORRY,外行~QQ

陳明谷
2015-08-27 20:01:12

像這種嗎

Adam Chen
2015-08-27 20:01:59

但是還是得3D列印出來才有辦法成形 然後把蠟做物體用耐火石膏圍住然後留一個澆注口 再加熱石膏模後把液態的蠟倒出 然後把液態的金屬灌入 冷卻後用破壞石膏模 拿出金屬物

Charlie Ting
2015-08-27 20:04:54

不需要精度的東西用 CAD/CAM 作的成本太高

林祐德
2015-08-27 20:07:24

好專業~嘖嘖嘖,改天我也來燒鋁來玩。。。

曾俊維
2015-08-27 20:22:31

不知那個蠟的料要去那買呢?

Clarence Lee
2015-08-27 21:02:56

文中就有啦... 3dmart本身就是賣材料的廠商了...

Adam Chen
2015-08-27 21:27:39

露天他們有賣 但是價格和普通線材比不便宜

麥麥
2015-08-27 22:07:45

印的時候,旁邊放一台工業用電風扇~~應該就可以冷卻了


原文網址 Roy Lo
2015-08-27 01:20:06

就是那個光~!

Roy Lo
2015-08-27 01:29:24

Roy Lo
2015-08-27 01:29:35

Charlie Ting
2015-08-27 01:29:49

照了什麼光?

Roy Lo
2015-08-27 01:29:50

Roy Lo
2015-08-27 01:30:19

手電筒而已, 哈~

Roy Lo
2015-08-27 01:30:35

張不凡
2015-08-27 03:32:16

鐵塔蠟燭?


 

發文排行榜

回文排行榜

熱門關鍵字